Glycol-compatible silicone hose for EV battery loops, energy storage and data-centre cooling. Low permeation, high dielectric strength, and a wall that survives a 15-year thermal cycle.
A battery cooling circuit runs hot ethylene glycol at 60–80 °C for a decade, with pressure pulses from the pump and vibration from the road. Silicone is chosen over EPDM because it keeps its flexibility at −40 °C and does not harden into a brittle pipe, but only if the compound is formulated for glycol rather than water.
The two numbers that decide a programme are permeation and the joint. Glycol loss through the wall shows up as a slow coolant drop nobody can find; a clamp that relaxes shows up as a leak at the cold end of a thermal cycle. We specify a glycol-resistant compound and a wall thickness that keeps permeation inside the OEM limit, then qualify the assembly with a thermal shock test rather than the hose alone.
Same compound family, different construction. Mixing two options on one order is common and usually cheaper than splitting the purchase.
Formed and straight runs inside the pack
Rack-level coolant distribution
Pressure and abrasion resistance
UL 94 V-0 for enclosed electronics
Module and pack-level coolant loops with formed routing.
Containerised BESS thermal management, outdoor rated.
Rack manifold hose with quick-connect ends.
Liquid-cooled cable and connector circuits.
Inverter and IGBT cold-plate connections.
Coolant loops with deionised water and glycol blends.
Permeation is measured on a 1 m loop at 80 °C with a 50/50 glycol-water mix. Values are for the hose only; a clamped assembly adds joint loss.
| ID (mm) | OD (mm) | Wall (mm) | Working (bar) | Permeation | Dielectric |
|---|---|---|---|---|---|
| 6 | 12 | 3.0 | 5 | low | > 20 kV/mm |
| 8 | 15 | 3.5 | 5 | low | > 20 kV/mm |
| 10 | 18 | 4.0 | 4 | low | > 20 kV/mm |
| 13 | 22 | 4.5 | 4 | medium | > 20 kV/mm |
| 16 | 26 | 5.0 | 3 | medium | > 20 kV/mm |
| 19 | 30 | 5.5 | 3 | medium | > 20 kV/mm |
| 25 | 38 | 6.5 | 3 | medium | > 20 kV/mm |
STEP file, glycol mix, operating temperature and the coolant loss your programme allows. We come back with a wall thickness and a formed-hose proposal, plus a thermal shock test plan for the assembly.